Introduction to the Advantages of Mobile Laboratories

1. Small Footprint: The mobile container-based PCR laboratory, constructed from a standard shipping container, features experimental workflows and equipment designed according to standard laboratory protocols. It is also equipped with a decontamination room in accordance with the requirements of T/CECS662G-2020, the "Technical Standards for Construction of Biosafety Level 2 Laboratories for Medical Use." The total footprint is approximately 52.5 square meters, making it suitable for placement in virtually any medical facility or outbreak area. In emergency situations, it can be used as a vehicle-mounted laboratory and, once transported to the outbreak site, can be put into operation immediately without any additional installation.

2021-11-03

The asphalt penetration tester features a high degree of automation.

1. The product is fully computerized and automated; experimental results are automatically calculated, eliminating the frustration of manual calculations for customers.

2021-10-31

Precautions and Instructions for Use of the Asphalt Mixture Compaction Tester

1. First, connect the three plugs at the back of the cabinet properly. The “motor” should be connected to the motor input port on the cabinet, the “non-contact proximity switch” should be connected to the counting port, and the “power supply” should be connected to the power port. At the same time, make sure the neutral wire is properly connected.

2021-10-28

Operating Procedures for the Asphalt Softening Point Tester

■Place the metal ring on a glass plate coated with a glycerin-talc powder release agent (glycerin:talc powder = 2:1). Heat the asphalt (for petroleum asphalt, heat to ≤ the estimated softening point + 90℃; for coal asphalt, heat to ≤ the estimated softening point + 50℃), stir it thoroughly, sieve it, and then pour it into the metal ring so that its surface slightly exceeds the top of the ring.

2021-10-25

Introduction to the Parameters of the Asphalt Extensometer

This test is applicable for evaluating the elastic recovery performance of thermoplastic rubber-modified asphalt polymers—that is, determining the percentage of deformation recovery through the sieve holes after the specimen has been elongated to a specified length using a ductility tester. Supplied by Hebei Dahong Testing Instrument Co., Ltd. Unless otherwise specified, the test temperature is 25℃, and the tensile rate is 5 cm/min ± 0.25 cm/min.